| Characteristic (UOM) |
Test Method |
Minimum Text Value | ||||
| XLN | LN | MN | HN | XHN | ||
| Mass Per Unit Area (GSM) | 7016 Part-1 | 35, 55, 60 | 70 | 120 | 200 | 300 |
| Tensile Strength at Break LD (Kg/Cm2) | IS:13360 | >250 | >250 | >250 | >250 | >250 |
| Tensile Strength at TD (Kg/Cm2) | IS:13360 | >200 | >200 | >200 | >200 | >200 |
| Elongation at Break LD (%) | IS:13360 | >300 | >400 | >400 | >400 | >400 |
| Elongation at Break TD (%) | IS:13360 | >250 | >300 | >300 | >300 | >300 |
| Tear Strength (Elmendorf) LD (Gram) | IS:14611, Annex F | >650 | >1200 | >2080 | >3200 | >4000 |
| Tear Strength (Elmendorf) TD (Gram) | IS:14611, Annex F | >450 | >900 | >1600 | >2800 | >3500 |
| Free Fall Dart Impact (Gram) | IS:13360 | >100 | >250 | >400 | >700 | >800 |
| AcceleratedUVResistance - After 192 Hrs of Aging (%) | IS:14622, AnnexG | 70% to 50% from the Original Strength | ||||
| Definition | LD-LongitudinalDirection alsoKnownasMD-MachineDirection TD- TransverseDirectionalsoknownasOD–ppositeDirection |
|||||